DSM Stanyl? 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Cond)

Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic
Material Notes:
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:
- Highest mechanical properties at high temperatures
- Excellent resistance to wear and low friction
- Outstanding flow for easy processing and exceptional design freedom
- Stanyl High Flowgrades that match the best flowing LCPs while maintaining a high level of mechanical properties
Key Applications:
Information provided by DSM.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
| Physical Properties | Metric | English | Comments | |
|
|
||||
| Density | 1.77 g/cc | 0.0639 lb/in? | (DAM); ISO 1183 | |
| Water Absorption | 4.5 % | 4.5 % | DAM; Sim. to ISO 62 | |
| Moisture Absorption at Equilibrium | 1.3 % | 1.3 % | Humidity Absorption (DAM); Sim. to ISO 62 | |
| Linear Mold Shrinkage | 0.003 cm/cm | 0.003 in/in | Parallel (DAM); ISO 294-4 | |
| Linear Mold Shrinkage, Transverse | 0.009 cm/cm | 0.009 in/in | Parallel (DAM); ISO 294-4 | |
Mechanical Properties |
||||
|
|
||||
| Tensile Strength at Break | 130 MPa | 18900 psi | ISO 527-1/-2 | |
| Elongation at Break | 2.5 % | 2.5 % | ISO 527-1/-2 | |
| Tensile Modulus | 12 GPa | 1740 ksi | ISO 527-1/-2 | |
| Charpy Impact Unnotched | 7 J/cm? | 33.3 ft-lb/in? | 23?C; ISO 179/1eU | |
| Charpy Impact, Notched, Low Temp | 1.2 J/cm? | 5.71 ft-lb/in? | -30?C; ISO 179/1eA | |
| Charpy Impact, Notched | 1.4 J/cm? | 6.66 ft-lb/in? | 23?C; ISO 179/1eA | |
| Tensile Creep Modulus, 1000 hours | 9500 MPa | 1.38e+006 psi | ISO 899-1 | |
Electrical Properties |
||||
|
|
||||
| Volume Resistivity | 1e+010 ohm-cm | 1e+010 ohm-cm | IEC 60093 | |
| Surface Resistance | 1e+014 ohm | 1e+014 ohm | IEC 60093 | |
| Dielectric Strength | 20 kV/mm | 508 kV/in | IEC 60243-1 | |
| Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A | |
| Comparative Tracking Index | 350 V | 350 V | IEC 60112 | |
Thermal Properties |
||||
|
|
||||
| Melting Point | 295 ?C | 563 ?F | 10?C/min (DAM); ISO 11357-1/-3 | |
| UL RTI, Electrical | 140 ?C | 284 ?F | 0.75 mm; UL746B | |
| UL RTI, Electrical | 140 ?C | 284 ?F | 1.5 mm; UL746B | |
| UL RTI, Mechanical with Impact | 110 ?C | 230 ?F | 0.75 mm; UL746B | |
| UL RTI, Mechanical with Impact | 125 ?C | 257 ?F | 1.5 mm; UL746B | |
| UL RTI, Mechanical without Impact | 120 ?C | 248 ?F | 0.75 mm; UL746B | |
| UL RTI, Mechanical without Impact | 125 ?C | 257 ?F | 1.5 mm; UL746B | |
Descriptive Properties |
||||
|
|
||||
| Flame Retardant | Yes | |||
| Flame Retarding Agent | Yes | |||
| Heat Stabilized or Stable to Heat | Yes | |||
| Injection Molding | Yes | |||
| Lubricants | Yes | |||
| Platable | Yes | |||
| Release Agent | Yes | |||
| With Fillers | Yes | |||
|
|
||||
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.